The loaded carbon is recovered via a carbon recovery screen and treated in the elution and electrowinning circuit.Loaded carbon is acid washed with dilute hydrochloric acid in an 18 t acid wash column prior to transfer into an elution column where it is presoaked in a cyanidecaustic solution for 30 minutes to elute gold.